primeweld tig225x banner 2

sanitary weld - inside corner.

by RJ (shopdog)
(DePere, WI)

I TIG'ed some stainless salt pans for a food service company and I backed the corners with aluminum angle. Turned out real nice. Even though the job didn't require it yet,I would like to be ready to provide a nicely finished (NFS sanitary type) inside corner. I have a feeling they will be asking for it in the future. I run a Synchrowave 250 and use 2% lanthanted and 2% ceriated.
BTW smokin' site!

--------------------------------------------------

you can convert your aluminum angle to backing plates by drilling a bunch of holes to provide a path for argon. and then use some tubing on the back side also with a bunch of holes drilled on the back side along with some jb weld or devcon putty.

Return to tig forum.

Enjoy this page? Please pay it forward. Here's how...

Would you prefer to share this page with others by linking to it?

  1. Click on the HTML link code below.
  2. Copy and paste it, adding a note of your own, into your blog, a Web page, forums, a blog comment, your Facebook account, or anywhere that someone would find this page valuable.