structual welding test

by caleb giegerich
(dubuque, ia)

hello everybody,

i have a welding certification test coming up soon. its 1" thick material V-groove in flat position 1/4" root opening w/ a backer GMAW i believe the shielding gas is 98/2. It will be ultrasonically tested and bent. Looking for weld techniques for the root pass, really the only concern that i have for the test. Should i make cursive e's, run it straight thru?? feedback would be appreciated!!!


Jody here from weldingtipsandtricks

make sure to push the puddle and keep the wire on the leading edge of the puddle.
I would trace the front edge of the puddle on the root.

anyone else got any tips?